CCS25 Cu Co Sn Prealloyed Hmoov rau Zoo Marble Pom Hniav
CCS25 Cu Co Sn Prealloyed Hmoov rau Zoo Marble Pom Hniav
1. Pre-alloyed hmoov yog dab tsi
Pre-alloyed hmoov yog ib qho nyuaj, tsawg compressible thiab li no yuav tsum tau ntau dua nias loads los tsim high density compacts.Txawm li cas los xij, lawv muaj peev xwm ua tau cov khoom muaj zog sintered.Pre-alloying kuj tseem siv tau thaum tsim cov khoom siv homogeneous los ntawm cov hmoov nplej yuav tsum muaj qhov kub thiab txias thiab ntev sintering lub sij hawm.Cov piv txwv zoo tshaj plaws yog cov hlau tsis muaj hlau, uas nws cov ntsiab lus chromium thiab npib tsib xee yuav tsum tau ua ntej-alloyed kom muaj kev lag luam tsim los ntawm hmoov metallurgy.
2. Cov Parameters ntawm CCS25
Lub ntsiab lus | Cu, Co, Sn | |
Theoretical ntom ntom | 8.29 g / cm³ | |
Sintering kub | 760 ℃ | |
Khoov zog | 800 Mpa | |
Hardness | 85-95 HWB |
3. CCS25 Pre-alloyed Powder Cim
- Sintered Structure ntawm cov khoom yog ib yam, zoo thiab compact, lub pob zeb diamond yog wetted thiab mechanically qhwv.Lub cim tseem ceeb ntawm daim ntawv cog lus yog "Tough & Friagility", zoo hnav tsis kam thiab kev ua haujlwm zoo.
- Siv rau nruab nrab kom zoo marble hniav, iav sib tsoo log.
4. Kev qhia siv rau Mrable Saw Hniav
- Hlau hmoov
- 50-70% CCS25
- + 25-35% kub
- + 4-7% Sn
B. Pob Zeb Diamond
- 50/60 @ 30%
- 60/70 @ 40%
- 70/80 @ 30%
- Pob zeb diamond concentration @ 20-25%
C. Sintering kub 760-780 ℃